HDPE geomembrane 0.5mm(for pond lining)
HDPE geomembrane 0.5mm(for pond lining), 1. thickness:0.1-3mm, 2. width: 1-8m, 3. length:50m-200m, 4.color:black... - details see: https://www.buildingsupplieshub.com/hdpe-geomembrane-0-5mm-for-pond-lining-10057774
| Type: Geomembranes,geomembrane | Place of Origin: Shandong China (Mainland) | Brand Name: dageng | Material: HDPE,LDPE |
HDPE geomembrane 1.5mm
Geomembrane Introduction:
HDPE GeoMembraneis the most widely used geosynthetic liner today. Pond Liner enjoys particularly high acceptance in the pond construction.
Geomembrane Usage:
HDPE Geo Membrane is mostly used for solid waste containment (e.g. sanitary land fill), mining, and water containment applications (e.g. lagoon and water reservoir).
Technical Parameters:
No. | Item | Test Value | ||||||
| 0.75mm | 1.0 mm | 1.25 mm | 1.5 mm | 2.0 mm | 2.5 mm | 3.0mm | ||
| 1 | Minimum Density(g/cm³) | 0.939 | ||||||
| 2 | Tensile Property | |||||||
| Strength at yield,N/mm | 11 | 15 | 18 | 22 | 29 | 37 | 44 | |
| Strength at break ,N/mm | 20 | 27 | 33 | 40 | 53 | 67 | 80 | |
| Elongation at yield,% | 12 | |||||||
| Elongation at break,% | 700 | |||||||
| 3 | Tear Resistance N | 93 | 125 | 156 | 187 | 249 | 311 | 374 |
| 4 | Puncture Resistance N | 240 | 320 | 400 | 480 | 640 | 800 | 960 |
| 5 | Stress Crack Resistance, hrs | 300 | ||||||
| 6 | Carbon Black | |||||||
| Carbon Black Content, % | 2.0-3.0 | |||||||
| Carbon Black Dispersion | 1 or 2 | |||||||
| 7 | Oxidation Induction Time(OTI) | |||||||
| Standard OTI Min | 100 | |||||||
| High Pressure OTI Min | 400 | |||||||
| 8 | Impact Cold Crack at -70°C | Pass | ||||||
| 9 | Water vapor permeability (g.cm/cm2 .s.Pa) | ≤1.0×10-16 | ||||||
| 10 | Dimensional Stability (%) | ±2 | ||||||
| Packaging Detail:according to customer's needs |